Majic 1 gal. Red Oxide Tractor Truck & Implement Enamel Primer
$64.99
Majic 1 gal. Red Oxide Tractor Truck & Implement Enamel Primer
Majic 1 gal. Red Oxide Tractor Truck & Implement Enamel Primer
Item # 103095399
Add this item to unlock free delivery!
Notice:
This Item cannot be shipped to CA.Get everything you need
Neighbor’s Club Members earn points with purchases.
Add this item to unlock free delivery!
Shopping at
Grassland (franklin) TN
Delivery to
Free standard delivery on online footwear & Clothing purchases of $49 and over.
Notice:
This Item cannot be shipped to CA.Get everything you need
Neighbor’s Club Members earn points with purchases.
Majic Tractor Truck & Implement Enamel Primer is a durable, heavy-duty, rust-inhibitive, alkyd primer specifically formulated for excellent adhesion, and resistance to weathering and corrosion. The auto primer paint may be applied by brush, roll or spray to iron, steel and aluminum surfaces.
- Heavy-duty, rust-inhibitive alkyd primer
- Specially formulated for excellent adhesion and resistance to weathering and corrosion
- Auto primer paint may be applied by brush, roll or spray
- Can be applied to iron, steel and aluminum surfaces
- Red oxide primer color
| Brand | Majic |
|---|---|
| Country of Origin | Made in USA |
| Container Size | 1 gal. |
| Coverage Area | 600-700 sq. ft./gal. |
| Dry to Touch | 5-10 hours |
| Features | Heavy-duty, rust-inhibitive alkyd primer. Specially formulated for excellent adhesion and resistance to weathering and corrosion. Auto primer paint may be applied by brush, roll or spray. Can be applied to iron, steel and aluminum surfaces |
| Finish | None |
| Interior and/or Exterior Use | Exterior |
| Package Quantity | 2 |
| Paint Base | Enamel |
| Surface Compatibility | Vehicle Surfaces |
| Primary Color | Red |
| Recommended Number Of Coats | 2 |
| Time Before Recoating | 24 hours |
| VOC Content | 250 g/L |
| Warranty | None |
| Manufacturer Part Number | 8-2989-1 |
Have a question?
Start typing your question and we'll check if it was already asked and answered.
1 - 10 of 15 Questions
Newest questions
Q: How soon can it be sanded
a month ago1 Answer
- A: Hi Nick, You can sand this primer after waiting 24 hours. Reviewers have noted that the primer becomes rock hard after this time, though others found it may remain soft for several days if not mixed with a hardener and reducer as recommended.a month agoHelpful?
Q: Can you spray acrylic enamel paint over majic oil-base primer.?
a year ago1 Answer
- A: Hello Booboo, yes, you can apply enamel paint to an oil-based primer so long as you allow the primer to properly and completely dry before application.a year agoHelpful?
Q: Can you use hardener with magic primer
2 years ago1 Answer
- A: Majic Catalyst Hardener can be used with this paint.2 years agoHelpful?
Q: Recommend reducer for manic red oxide primer
2 years ago1 Answer
- A: For best results, I would recommend thinning Majic T&I Red Oxide Primer with Majic Reducer, #8-0750, (SKU: 117711999) at a ratio of approximately 10%, apply in thin coats and allow 24 hours to dry before applying additional coats of primer, or top-coating with a finish enamel.2 years agoHelpful?
Q: can it be used on fiberglass
4 years ago1 Answer
- A: This product is formulated to be used on iron, steel, aluminum, and properly primed galvanized metal, not fiberglass.4 years agoHelpful?
Q: mixing ratio of hardener to a gallon of paint?
4 years ago1 Answer
- A: For additional product support, please contact 1 (800) 624-42524 years agoHelpful?
Q: Will this primer adhere to galvanized roof panels?
6 years ago1 Answer
- A: Majic Tractor, Truck & Implement Primers (Red Oxide, or Sandable Gray) are industrial oil/alkyd coatings that are designed for, and provide excellent adhesion & protection to ferrous metal surfaces – Not recommended for galvanized surfaces. To Paint galvanized panels with Majic T&I Enamels, galvanized surfaces must be cleaned and solvent wiped (to remove surface oils), etched/profiled with an acid based metal prep solution, then primed with an appropriate galvanized metal primer (non-cementitious), or a compatible self-etching primer, in accordance to manufacturer’s application & re-coat instructions.6 years agoHelpful?
Q: can majic applied over apoxy primer
6 years ago1 Answer
- A: Majic Tractor, Truck & Implement Primers and Enamels are high quality, hard-drying alkyds that exhibit excellent adhesion, corrosion resistance and protection to surfaces subjected to hard use, and harsh exposures… While Majic T&I Enamels are designed for use over Majic T&I Primers, painting either over a properly prepared epoxy primer should pose no problems (though adhesion testing is strongly recommended). The epoxy primer must be clean, dry and free of chalk, dirt, grease/oils, or other surface contaminants that may interfere with the adhesion of Majic T&I Products – and light sanding of the epoxy primer would be recommended to create a “profile” for a better, stronger, mechanical bond between 2 product films. Please carefully read, and follow, all label directions regarding application of Majic T&I Products, with special attention paid to the recommended applied thickness of each coating (thin applications @ 2.5 – 3.0 mils wet), and the allowable re-coat times for each (minimum 24 hours between coats). Too heavy an application, and/or re-coating too soon will result in a film that won’t dry “hard” for several days…or longer.6 years agoHelpful?
Q: Do I need to sand between each coat ? What about if I use the primer, will it need to be sanded also ?
7 years ago1 Answer
- A: Because these are oil/alkyd products, it is always good practice to sand between coats with a very fine grit paper (recommended 350 grit), or fine Scotch Brite pad. Light sanding not only removes surface irregularities (such as dust that may have settled on the surface during drying), but also aids in inter-coat adhesion, and helps to maintain a uniform & consistent finish application.7 years agoHelpful?
Q: Hi If I'm going to use a brush to apply the primer - do I need to thin the primer or put it on just like it is in the can - once mixed properly ???
7 years ago1 Answer
- A: To apply Majic T&I Red Oxide Primer by brush, first mix the contents of the gallon, thoroughly, until the product is a smooth and uniform consistency. Then, for best results, I would recommend thinning Majic T&I Red Oxide Primer with Majic Reducer, #8-0750, at a ratio of approximately 10%, apply in thin coats and allow 24 hours to dry before applying additional coats of primer, or top-coating with a finish enamel. The purpose for reduction is to help manage/control the recommended application thickness, and to aid in the “flow & leveling” of the applied film (too heavy an application, and/or re-coating too soon may result in a film that won’t dry “hard” for several days or longer).7 years agoHelpful?
1 - 10 of 15 Questions
Q&As
Have a question?
Start typing your question and we'll check if it was already asked and answered.
1 - 10 of 15 Questions
Newest questions
Q: How soon can it be sanded
a month ago1 Answer
- A: Hi Nick, You can sand this primer after waiting 24 hours. Reviewers have noted that the primer becomes rock hard after this time, though others found it may remain soft for several days if not mixed with a hardener and reducer as recommended.a month agoHelpful?
Q: Can you spray acrylic enamel paint over majic oil-base primer.?
a year ago1 Answer
- A: Hello Booboo, yes, you can apply enamel paint to an oil-based primer so long as you allow the primer to properly and completely dry before application.a year agoHelpful?
Q: Can you use hardener with magic primer
2 years ago1 Answer
- A: Majic Catalyst Hardener can be used with this paint.2 years agoHelpful?
Q: Recommend reducer for manic red oxide primer
2 years ago1 Answer
- A: For best results, I would recommend thinning Majic T&I Red Oxide Primer with Majic Reducer, #8-0750, (SKU: 117711999) at a ratio of approximately 10%, apply in thin coats and allow 24 hours to dry before applying additional coats of primer, or top-coating with a finish enamel.2 years agoHelpful?
Q: can it be used on fiberglass
4 years ago1 Answer
- A: This product is formulated to be used on iron, steel, aluminum, and properly primed galvanized metal, not fiberglass.4 years agoHelpful?
Q: mixing ratio of hardener to a gallon of paint?
4 years ago1 Answer
- A: For additional product support, please contact 1 (800) 624-42524 years agoHelpful?
Q: Will this primer adhere to galvanized roof panels?
6 years ago1 Answer
- A: Majic Tractor, Truck & Implement Primers (Red Oxide, or Sandable Gray) are industrial oil/alkyd coatings that are designed for, and provide excellent adhesion & protection to ferrous metal surfaces – Not recommended for galvanized surfaces. To Paint galvanized panels with Majic T&I Enamels, galvanized surfaces must be cleaned and solvent wiped (to remove surface oils), etched/profiled with an acid based metal prep solution, then primed with an appropriate galvanized metal primer (non-cementitious), or a compatible self-etching primer, in accordance to manufacturer’s application & re-coat instructions.6 years agoHelpful?
Q: can majic applied over apoxy primer
6 years ago1 Answer
- A: Majic Tractor, Truck & Implement Primers and Enamels are high quality, hard-drying alkyds that exhibit excellent adhesion, corrosion resistance and protection to surfaces subjected to hard use, and harsh exposures… While Majic T&I Enamels are designed for use over Majic T&I Primers, painting either over a properly prepared epoxy primer should pose no problems (though adhesion testing is strongly recommended). The epoxy primer must be clean, dry and free of chalk, dirt, grease/oils, or other surface contaminants that may interfere with the adhesion of Majic T&I Products – and light sanding of the epoxy primer would be recommended to create a “profile” for a better, stronger, mechanical bond between 2 product films. Please carefully read, and follow, all label directions regarding application of Majic T&I Products, with special attention paid to the recommended applied thickness of each coating (thin applications @ 2.5 – 3.0 mils wet), and the allowable re-coat times for each (minimum 24 hours between coats). Too heavy an application, and/or re-coating too soon will result in a film that won’t dry “hard” for several days…or longer.6 years agoHelpful?
Q: Do I need to sand between each coat ? What about if I use the primer, will it need to be sanded also ?
7 years ago1 Answer
- A: Because these are oil/alkyd products, it is always good practice to sand between coats with a very fine grit paper (recommended 350 grit), or fine Scotch Brite pad. Light sanding not only removes surface irregularities (such as dust that may have settled on the surface during drying), but also aids in inter-coat adhesion, and helps to maintain a uniform & consistent finish application.7 years agoHelpful?
Q: Hi If I'm going to use a brush to apply the primer - do I need to thin the primer or put it on just like it is in the can - once mixed properly ???
7 years ago1 Answer
- A: To apply Majic T&I Red Oxide Primer by brush, first mix the contents of the gallon, thoroughly, until the product is a smooth and uniform consistency. Then, for best results, I would recommend thinning Majic T&I Red Oxide Primer with Majic Reducer, #8-0750, at a ratio of approximately 10%, apply in thin coats and allow 24 hours to dry before applying additional coats of primer, or top-coating with a finish enamel. The purpose for reduction is to help manage/control the recommended application thickness, and to aid in the “flow & leveling” of the applied film (too heavy an application, and/or re-coating too soon may result in a film that won’t dry “hard” for several days or longer).7 years agoHelpful?
1 - 10 of 15 Questions
Similar Items
Items You May Like
Reviews
5 to 8 of 9 Reviews .
1 – 4 of 9 Reviews
Most Recent
Ohio
Reviews 3
5 out of 5 stars.
Excellent product, tough durable system !
7 years ago
I used Majic red oxide primer on a dump bed.
I called Majic multiple times and they were great ! Walked me through it step by step.
I sanded metal and did a phosphoric acid wash and let set overnight .
Rinse let dry and used a Wagner type sprayer, sprayed primer.
Let primer dry overnight then light sanded, blow off dust with air then sprayed Majic tractor & implement paint.
2 light coats then 3rd coat with hardener.
Been 2 years now and still looks great !
Highly recommended >Great customer service.
SweepstakesYes
Yes, I recommend this product.
Reviews 2
1 out of 5 stars.
Where was this can at?
8 years ago
This gallon must have been sitting for a long,long time. All the pigment was like thick, heavy mud sitting on the bottom. It had to take me an hour to stir and break up the sediment on the bottom
Greeley, CO, United States
Reviews 2
1 out of 5 stars.
Junk
9 years ago
Horrible product I bought it shook it up the product is so hard you cannot even Stir It with a stir stick
No, I do not recommend this product.
Asheville, NC, United States
Review 1
5 out of 5 stars.
Great
11 years ago
I have read good and bad reviews about this brand. I went to their website and mixed the hardener and reducer like they recommend and sanded the metal. Sprayed great and after 24 hours rock hard, and looks great to be a primer. Very happy with it, think others had problems because not mixing right.
Yes, I recommend this product.